Identificador persistente para citar o vincular este elemento: http://hdl.handle.net/10553/112528
Título: In Vitro Testing of 2 Adjustable-Loop Cortical Suspensory Fixation Systems Versus Interference Screw for Anterior Cruciate Ligament Reconstruction
Autores/as: Garcés Martín, Gerardo 
Martel Fuentes, Oscar 
Yánez Santana, Manuel Alejandro 
Manchado Herrera, Ignacio 
Motta Da Rocha, Luci Mara 
Clasificación UNESCO: 321315 Traumatología
Palabras clave: Biomechanical testing
Anterior cruciate ligament reconstruction
Suspensory fixation
Interference screw
Fecha de publicación: 2021
Publicación seriada: Orthopaedic Journal of Sports Medicine 
Resumen: Background: It is not clear whether the mechanical strength of adjustable-loop suspension devices (ALDs) in anterior cruciate ligament (ACL) reconstruction is device dependent and if these constructs are different from those of an interference screw. Purpose: To compare the biomechanical differences of 2 types of ALDs versus an interference screw. Study Design: Controlled laboratory study. Methods: ACL reconstruction was performed on porcine femurs and bovine extensor tendons with 3 types of fixation devices: interference screw, UltraButton (UB) ALD, and TightRope (TR) ALD (n = 10 for each). In addition to specimen testing, isolated testing of the 2 ALDs was performed. The loading protocol consisted of 3 stages: preload (static 150 N load for 5 minutes), cyclic load (50-250 N at 1 Hz for 1000 cycles), and load to failure (crosshead speed 50 mm/min). Displacement at different cycles, ultimate failure load, yield load, stiffness, and failure mode were recorded. Results: In specimen testing, displacement of the ALDs at the 1000th cycle was similar (3.42 ± 1.34 mm for TR and 3.39 ± 0.92 mm for UB), but both were significantly lower than that of the interference screw (7.54 ± 3.18 mm) (P <.001 for both). The yield load of the UB (547 ± 173 N) was higher than that of the TR (420 ± 72 N) (P =.033) or the interference screw (386 ± 51 N; P =.013), with no significant difference between the latter 2. In isolated device testing, the ultimate failure load of the TR (862 ± 64 N) was significantly lower than that of the UB (1879 ± 126 N) (P <.001). Conclusion: Both ALDs showed significantly less displacement in cyclic loading at ultimate failure than the interference screw. The yield load of the UB was significantly higher than that of the other 2. The ultimate failure occurred at a significantly higher load for UB than it did for TR in isolated device testing. Clinical Relevance: Both UB and TR provided stronger fixation than an interference screw. Although difficult to assess, intrinsic differences in the mechanical properties of these ALDs may affect clinical outcomes.
URI: http://hdl.handle.net/10553/112528
ISSN: 2325-9671
DOI: 10.1177/23259671211031652
Fuente: Orthopaedic Journal of Sports Medicine [ISSN 2325-9671], v. 9 (9), (Septiembre 2021)
Colección:Artículos
Adobe PDF (278,45 kB)
Vista completa

Google ScholarTM

Verifica

Altmetric


Comparte



Exporta metadatos



Los elementos en ULPGC accedaCRIS están protegidos por derechos de autor con todos los derechos reservados, a menos que se indique lo contrario.